Enzymatic, urease-mediated mineralization of gellan gum hydrogel with calcium carbonate, magnesium-enriched calcium carbonate and magnesium carbonate for bone regeneration applications.

Douglas, Timothy Edward Lim and Lapa, Agata and Samal, Sangram and Declercq, Heidi and Declercq, Heidi and Schaubroeck, David and Mendes, Ana and Van der Voort, Pascal and Dokupil, Agnieszka and Plis, Agnieszka and De Schamphelaere, Karel and Chronakis, Ioannis and Pamula, Elzbieta and Skirtach, Andre (2017) Enzymatic, urease-mediated mineralization of gellan gum hydrogel with calcium carbonate, magnesium-enriched calcium carbonate and magnesium carbonate for bone regeneration applications. Journal of Tissue Engineering and Regenerative Medicine. pp. 3556-3566. ISSN 1932-6254

[thumbnail of s1-ln24061701993758110-1939656818Hwf-961200449IdV38594067824061701PDF_HI0001]
Preview
PDF (s1-ln24061701993758110-1939656818Hwf-961200449IdV38594067824061701PDF_HI0001)
s1_ln24061701993758110_1939656818Hwf_961200449IdV38594067824061701PDF_HI0001.pdf - Accepted Version

Download (2MB)

Abstract

Mineralization of hydrogel biomaterials is considered desirable to improve their suitability as materials for bone regeneration. Calcium carbonate (CaCO3) has been successfully applied as a bone regeneration material, but hydrogel‐CaCO3 composites have received less attention. Magnesium (Mg) has been used as a component of calcium phosphate biomaterials to stimulate bone‐forming cell adhesion and proliferation and bone regeneration in vivo, but its effect as a component of carbonate‐based biomaterials remains uninvestigated. In the present study, gellan gum (GG) hydrogels were mineralized enzymatically with CaCO3, Mg‐enriched CaCO3 and magnesium carbonate to generate composite biomaterials for bone regeneration. Hydrogels loaded with the enzyme urease were mineralized by incubation in mineralization media containing urea and different ratios of calcium and magnesium ions. Increasing the magnesium concentration decreased mineral crystallinity. At low magnesium concentrations calcite was formed, while at higher concentrations magnesian calcite was formed. Hydromagnesite (Mg5(CO3)4(OH)2.4H2O) formed at high magnesium concentration in the absence of calcium. The amount of mineral formed and compressive strength decreased with increasing magnesium concentration in the mineralization medium. The calcium:magnesium elemental ratio in the mineral formed was higher than in the respective mineralization media. Mineralization of hydrogels with calcite or magnesian calcite promoted adhesion and growth of osteoblast‐like cells. Hydrogels mineralized with hydromagnesite displayed higher cytotoxicity. In conclusion, enzymatic mineralization of GG hydrogels with CaCO3 in the form of calcite successfully reinforced hydrogels and promoted osteoblast‐like cell adhesion and growth, but magnesium enrichment had no definitive positive effect.

Item Type:
Journal Article
Journal or Publication Title:
Journal of Tissue Engineering and Regenerative Medicine
Uncontrolled Keywords:
/dk/atira/pure/subjectarea/asjc/2200/2204
Subjects:
?? hydrogel gellan gumcarbonate mineralization magnesium composite enzymebiomedical engineeringbiomaterialsmedicine (miscellaneous) ??
ID Code:
125415
Deposited By:
Deposited On:
05 Jun 2018 07:32
Refereed?:
Yes
Published?:
Published
Last Modified:
09 Jan 2024 00:21